Products

  • Hastelloy C-276 MATERIAL DATA SHEETS

    HASTELLOY C276, UNS N10276 is considered the most versatile corrosion resistant nickel alloy available. Alloy C-276 also has excellent resistance to pitting, stress-corrosion cracking, especially suitable for use in high temperature, inorganic and organic acids mixed with impurities (such as formic acid and acetic acid), and seawater corrosive environments.

  • Monel 400 Uns N04400 W.Nr. 2.4360 And 2.4361

    MONEL nickel-copper alloy 400 (UNS N04400) is a solid-solution alloy that can be hardened only by cold working. It has high strength and toughness over a wide temperature range and excellent resistance to many corrosive environments. Alloy 400 is widely used in many fields, especially marine and chemical processing. Typical applications are valves and pumps; pump and propeller shafts; marine fixtures and fasteners; electrical and electronic components; springs; chemical processing equipment; gasoline and fresh water tanks; crude petroleum stills, process vessels and piping; boiler feed water heaters and other heat exchangers; and deaerating heaters.Chemical Compositions

  • Nimonic

    High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Cu Ti Al Co other no greater than Nimonic90 0.13 1 1 0.015 18~21 base ≤1.5 ≤0.2 2~3 1~2 15~21 lead≤0.002      B≤0.02        Zr≤0.15 Nimonic91 0.1 1 1 0.015 27~30 base ≤1 ≤0.5 1.9~2.7 0.9~1.5 19~21 Nb0.4~1.1  B0.002~0.01  Zr≤0.1 Alloy property minimum Grade state tensile strength RmN/m㎡ Yield Strength Rp0.2N/...
  • ALLOY 600 MATERIAL DATA SHEETS

    INCONEL  600

    Inconel Alloy 600 A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water, and caustic corrosion. Used for furnace components, in chemical and food processing, in nuclear engineering, and for sparking electrodes.

    UNS: N06600

    W.Nr.: 2.4816

  • High Temperature Alloy

    Application Chemistry Typical Carbon  0.080 max Manganese  2.00 max Silicon  0.75 max Chromium  24.00- 26.00 Nickel  19.00- 22.00 Molybdenum  0.75 max Phosphorus  0.040 max Physical Properties Density  0.29 lbs/in³ 9.01 g/cm³ Electrical Resistivity  microhm-in (microhm-cm)  68°F (20°C)  37.0 (94.0) Specific Heat  BTU/lb/°F (kJ/kg•K)  32-212°F (0-100°C)  0.12 (0.50) Thermal Conductivity  BTU/hr/ft²/ft/°F (W/m•K) At 212°F (100°C)  8....