Products
-
Alloy
High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Al Ti Cu Mo Nb other no greater than Inconel600 0.15 0.5 1 0.015 0.03 14~17 base 6~10 - - ≤0.5 - - - Inconel601 0.1 0.5 1 0.015 0.03 21~25 base 10~15 1~1.7 - ≤1 - - - Inconel625 0.1 0.5 0.5 0.015 0.015 20~23 base ≤5 ≤0.4 ≤0.4 - 8~10 3.15~4.15 Co≤1 Inconel725 0.03 0.2 0.35 0... -
ALLOY 625 MATERIAL DATA SHEETS
Alloy 625 is a nonmagnetic , corrosion – and oxidation-resistant, nickel-based alloy. Its outstanding strength and toughness in the temperature range cryogenic to 2000°F (1093°C) are derived primarily from the solid solution effects of the refractory metals, columbium and molybdenum, in a nickel-chromium matrix. The alloy has excellent fatigue strength and stress-corrosion cracking resistance to chloride ions. Some typical applications for alloy 625 have included heat shields, furnace hardware, gas turbine engine ducting, combustion liners and spray bars, chemical plant hardware, and special seawater applications.
-
HASTELLOY B2 UNS N10665 W.NR.2.4617
Hastelloy B2 is a solid solution strengthened, nickel-molybdenum alloy, with significant resistance to reducing environments like hydrogen chloride gas, and sulfuric, acetic and phosphoric acids. Molybdenum is the primary alloying element which provides significant corrosion resistance to reducing environments. This nickel steel alloy can be used in the as-welded condition because it resists the formation of grain-boundary carbide precipitates in the weld heat-affected zone.
This nickel alloy provides excellent resistance to hydrochloric acid at all concentrations and temperatures. In additions, Hastelloy B2 has excellent resistance to pitting, stress corrosion cracking and to knife-line and heat-affected zone attack. Alloy B2 provides resistance to pure sulfuric acid and a number of non-oxidizing acids.
-
Hastelloy
High Temperature Alloy Chemical composition Grade C P S Mn Si Ni Cr Co Cu Fe N Mo Al W V Ti other no greater than HastelloyB 0.05 0.04 0.03 1 1 base ≤1 ≤2.5 - 4~6 - 26~30 - - 0.2~0.4 - - HastelloyB-2 0.02 0.04 0.03 1 0.1 base ≤1 ≤1 - ≤2 - 26~30 - - - - HastelloyB-3 0.01 0.04 0.03 3 0.1 ≥65 1~3 ≤3 ≤0.2 1~3 - 27~32 ≤0.5 ≤3 ≤0.2 ≤0.2 - ... -
Hastelloy C-276 MATERIAL DATA SHEETS
HASTELLOY C276, UNS N10276 is considered the most versatile corrosion resistant nickel alloy available. Alloy C-276 also has excellent resistance to pitting, stress-corrosion cracking, especially suitable for use in high temperature, inorganic and organic acids mixed with impurities (such as formic acid and acetic acid), and seawater corrosive environments.
-
Monel 400 Uns N04400 W.Nr. 2.4360 And 2.4361
MONEL nickel-copper alloy 400 (UNS N04400) is a solid-solution alloy that can be hardened only by cold working. It has high strength and toughness over a wide temperature range and excellent resistance to many corrosive environments. Alloy 400 is widely used in many fields, especially marine and chemical processing. Typical applications are valves and pumps; pump and propeller shafts; marine fixtures and fasteners; electrical and electronic components; springs; chemical processing equipment; gasoline and fresh water tanks; crude petroleum stills, process vessels and piping; boiler feed water heaters and other heat exchangers; and deaerating heaters.Chemical Compositions
-
Nimonic
High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Cu Ti Al Co other no greater than Nimonic90 0.13 1 1 0.015 18~21 base ≤1.5 ≤0.2 2~3 1~2 15~21 lead≤0.002 B≤0.02 Zr≤0.15 Nimonic91 0.1 1 1 0.015 27~30 base ≤1 ≤0.5 1.9~2.7 0.9~1.5 19~21 Nb0.4~1.1 B0.002~0.01 Zr≤0.1 Alloy property minimum Grade state tensile strength RmN/m㎡ Yield Strength Rp0.2N/... -
ALLOY 600 MATERIAL DATA SHEETS
INCONEL 600
Inconel Alloy 600 A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water, and caustic corrosion. Used for furnace components, in chemical and food processing, in nuclear engineering, and for sparking electrodes.
UNS: N06600
W.Nr.: 2.4816
-
High Temperature Alloy
Application Chemistry Typical Carbon 0.080 max Manganese 2.00 max Silicon 0.75 max Chromium 24.00- 26.00 Nickel 19.00- 22.00 Molybdenum 0.75 max Phosphorus 0.040 max Physical Properties Density 0.29 lbs/in³ 9.01 g/cm³ Electrical Resistivity microhm-in (microhm-cm) 68°F (20°C) 37.0 (94.0) Specific Heat BTU/lb/°F (kJ/kg•K) 32-212°F (0-100°C) 0.12 (0.50) Thermal Conductivity BTU/hr/ft²/ft/°F (W/m•K) At 212°F (100°C) 8.... -
Nitronic
High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Mo Ti Cu Nb N other no greater than Nitronic50 0.06 1 4~6 0.03 0.04 20.5~23.5 11.5~13.5 base 1.5~3 - - 0.1~0.3 0.2~0.4 - Nitronic60 0.1 3.5~4.5 7~9 0.03 0.04 16~18 8~9 base — — — — 0.08~0.18 - Alloy property minimum Grade state tensile strength RmN/m㎡ Yield Strength Rp0.2N/m㎡ Elongation As% B... -
ALLOY 718 MATERIAL DATA SHEETS
Inconel Alloy 718 A precipitation-hardenable nickel-chromium alloy also containing significant amounts of iron, niobium, and molybdenum along with lesser amounts of aluminum and titanium. It combines corrosion resistance and high strength with outstanding weldability including resistance to postweld cracking. The alloy has excellent creep-rupture strength at temperatures to 1300°F (700°C). Used in gas turbines, rocket motors, spacecraft, nuclear reactors, pumps, and tooling. INCONEL alloy 718SPF™ is a special version of INCONEL alloy 718, designed for superplastic forming.
UNS: N07718
W.Nr.: 2.4668
-
High Precision Alloy
High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Mo Cu Fe Al Co Ti no greater than 1J50 0.03 0.15~0.3 0.3~0.6 0.02 0.02 - 49.5~50.5 - ≤0.2 base — — — 1J79 0.03 0.3~0.5 0.6~1.1 0.02 0.02 - 78.5~80.5 3.8~4.1 ≤0.2 base — — — 3J53 0.05 0.8 0.8 0.02 0.02 5.2~5.8 41.5~43 0.7~0.9 — base 0.5~0.8 — 2.3~2.7 4J29 0.03 0.3 0.5 0.02 0.02 ...